Home > Blog > How Gold CIL Leaching Works Step by Step

Contact Us

Mrs. Lily
Chat Now

Your inquiry content must be between 10 to 5000 characters

Please enter Your valid email address

Please enter a correct verification code.

How Gold CIL Leaching Works Step by Step

The gold cil leaching process is a continuous sequence in which gold is dissolved from ore and simultaneously captured on activated carbon. Because the two steps happen in the same tanks rather than in separate circuits, the process behaves differently from conventional cyanidation, and understanding why matters for anyone specifying or operating a plant.

This article walks through the circuit stage by stage, from ore preparation to the loaded carbon that leaves for elution, and sets out the variables that determine whether recovery meets the design figure.

1. Preparing the Ore for the Gold CIL Leaching Process

The first stage of the gold cyanidation steps is comminution to a size at which the gold is exposed to the cyanide solution. Unlike flotation, which needs mineral liberation, leaching only requires that the solution can reach the gold. In practice this means grinding to the point where the gold grains are exposed at the particle surface or are accessible through pores in the host rock.

Grind size is a compromise between recovery and cost. Finer grinding exposes more gold but consumes more power and creates fine material that is harder to handle in the downstream circuit. Most gold plants grind to a P80 somewhere between 75 and 150 microns, with the exact figure established by leach test work at several sizes.

Gravity recovery is often placed in the grinding circuit, ahead of leaching. Coarse free gold dissolves slowly, so capturing it early with a gravity concentrator removes a slow-dissolving fraction from the circuit and shortens the time gold is held in inventory. The gravity concentrate is upgraded and treated separately.

Grinding also affects the chemistry of the leach. Freshly ground surfaces are more reactive, and grinding media can introduce iron that consumes cyanide and oxygen. Where the ore contains significant sulphide, the grinding environment can lower dissolved oxygen before the pulp even reaches the leach tanks, so aeration capacity has to allow for it.

2. Leaching Chemistry and Gold Cyanidation Steps

The basic reaction behind the gold cyanidation steps is well established: in the presence of cyanide and oxygen, gold dissolves to form a soluble cyanide complex. Two things must therefore be supplied continuously, and both are frequently under-provided in practice. Cyanide is dosed as a reagent, while oxygen comes from air sparged into the tanks or, in some circuits, from oxygen enrichment.

gold cyanidation steps begin with the dissolution reaction itself, which is electrochemical. Oxygen is reduced at one part of the gold surface and cyanide complexes the gold at another, and the two half-reactions have to occur simultaneously for dissolution to proceed. If either is limited, the rate falls regardless of the other.

Dissolution rate therefore depends on cyanide concentration, dissolved oxygen, pH, temperature and the surface area of exposed gold. pH is normally held above about 10 to prevent the formation of hydrogen cyanide gas, which is both a safety hazard and a loss of reagent. Lime is the usual reagent for this purpose.

Several minerals interfere with the chemistry of the gold cyanidation steps. Copper minerals consume cyanide by forming their own complexes, and a copper content of even a few tenths of a percent can double cyanide consumption. Sulphide minerals consume both cyanide and oxygen as they oxidise. Arsenic and antimony species can form films on gold surfaces that slow dissolution, and carbonaceous material can adsorb dissolved gold before it reaches the added carbon.

VariableTypical operating rangeEffect if incorrectly set
pH10.0 to 11.0Below 10, hydrogen cyanide forms; above 11, lime consumption rises
Cyanide concentrationSet by test work, often 0.05 to 0.10 percentToo low slows dissolution; too high wastes reagent
Dissolved oxygenAbove roughly 6 to 8 parts per millionLimits dissolution regardless of cyanide level
Pulp densityCommonly 40 to 50 percent solidsToo thick impairs mixing and carbon suspension
TemperatureAmbient, faster above about 20 degreesCold pulp slows kinetics noticeably
Grind sizeP80 of 75 to 150 micronsCoarse leaves locked gold; fine raises cost

Henan Amill Machinery Equipment sizes leach tanks from test work kinetics and from the actual pulp density the plant will run, rather than from a nominal residence time, because residence time alone does not describe whether the gold has time to dissolve.

3. Gold Adsorption on Carbon Within the Leach Tanks

The defining feature of the CIL arrangement is that activated carbon is present in the leach tanks while dissolution is happening, so gold adsorption on carbon begins the moment gold enters solution. Dissolved gold is adsorbed onto the carbon almost as soon as it enters solution, which keeps the concentration of dissolved gold in the pulp very low.

Keeping that concentration low has a direct kinetic benefit. Because the dissolution reaction is driven by the difference between the gold concentration at the mineral surface and in the bulk solution, removing gold from solution maintains a steeper driving force and accelerates the overall rate. This is the main reason CIL can outperform a separate leach-and-adsorb arrangement on ores where the leach reaction is slow or where re-precipitation is a risk.

gold adsorption on carbon follows a loading relationship in which the carbon takes up gold until it approaches equilibrium with the solution. In a multi-stage tank train the carbon moves counter-current to the pulp, entering at the last tank and progressing toward the first, so that the carbon is progressively loaded as it meets progressively richer pulp. This counter-current movement is what allows a high final loading on the carbon and a low gold concentration in the tailings, and it is the key design idea behind gold adsorption on carbon.

Carbon concentration in each tank is the central controlled variable in gold adsorption on carbon. Too little carbon and the adsorption capacity in that stage is insufficient; too much and the carbon inventory and elution load both rise. Typical circuits maintain a carbon concentration in the range of 10 to 25 grams per litre, staged so that the first tanks carry more carbon than the last.

For gold adsorption on carbon, quality matters as much as quantity. Fresh carbon has a high internal surface area and adsorbs effectively, while carbon that has been through many cycles accumulates calcium carbonate scale and organic fouling and loses capacity. Regular regeneration in a kiln at high temperature burns off the organic fouling and restores much of the capacity.

Carbon retention screens prevent the carbon from leaving the tank with the pulp. Screen apertures must be smaller than the smallest carbon particle but large enough to pass the pulp without excessive head loss, and a worn or incorrectly sized screen is a common cause of carbon loss to tailings.

Amill Machinery Equipment supplies leach tanks with agitators and interstage screens designed for carbon suspension, and our engineers specify the carbon transfer and carbon concentration control system as part of the circuit rather than as separate ancillary items.

4. Oxygen, Agitation and Tank Configuration

Oxygen supply is often the limiting factor in the gold cyanidation steps and in the gold cil leaching process generally, and it is frequently the least well understood. Air is sparged into the base of each tank, and the oxygen transfer rate depends on the bubble size, the depth of the tank and the degree of mixing. Simply adding cyanide when recovery is low will not help if oxygen is the constraint.

Agitation serves three purposes at once: it suspends the solids, disperses the sparged air, and keeps the carbon in motion so that the adsorption surface is continuously renewed. Impeller selection therefore has to satisfy all three, which usually means a large-diameter impeller running at moderate speed rather than a small high-speed unit.

Tank configuration affects residence time distribution. Tanks in series behave closer to plug flow than a single large tank, which improves recovery because it avoids short-circuiting of pulp through the circuit. Most CIL circuits use four to eight tanks in series, with the number set by the kinetics and by the target recovery.

Aeration should be adjustable and measurable. Dissolved oxygen measurement at each tank allows the operator to see whether the circuit is oxygen-limited, and variable air flow lets the supply be matched to demand. A circuit with fixed air supply and no dissolved oxygen instrumentation is operating blind on one of its two critical reagents.

The leach train should also include provision for reagent addition at more than one point. Adding lime at the mill and cyanide at the first leach tank is common, but where the ore is variable, additional dosing points allow the operator to correct pH or cyanide concentration part-way through the train rather than accepting whatever conditions develop.

5. From Loaded Carbon to Doré

Loaded carbon leaving the adsorption train carries the gold and is transferred to the elution circuit. Before elution, the carbon is usually washed with acid to remove calcium and other base metal salts that would otherwise report to the eluate and complicate electrowinning.

Elution strips the gold from the carbon using a hot solution of caustic cyanide. The carbon is contacted with the eluant at elevated temperature, and the gold desorbs into solution. Elution efficiency is temperature and concentration dependent, and incomplete stripping leaves gold on the carbon that then returns to the adsorption circuit, where it raises the gold inventory and reduces the effective capacity of the carbon.

Eluate then passes to electrowinning, where the gold is deposited onto steel wool cathodes. Cell efficiency depends on the gold concentration in the eluate, the current density and the cell configuration, and poorly performing cells leave gold in the spent electrolyte that must be returned to the circuit rather than discarded.

The final step is smelting the calcined cathodes with fluxes to produce doré bars. Metal accounting across elution, electrowinning and smelting should reconcile closely with the gold entering the circuit on the loaded carbon, and a persistent gap usually indicates gold trapped in the circuit rather than lost.

Not long ago, a gold cil leaching process at a mid-sized operation was recovering about 86 percent against a design figure of 92 percent. Investigation found dissolved oxygen in the leach train was around 4 parts per million rather than the 7 assumed in design, and elution was leaving measurable gold on the regenerated carbon. Improving air distribution in the first two tanks and adjusting the elution temperature brought recovery to about 90 percent over the following months.

6. FAQ: Gold CIL Leaching

6.1 What is the difference between CIL and CIP?

In CIL, activated carbon is present in the leach tanks so that dissolution and adsorption happen simultaneously. In CIP, leaching is completed first and the pulp then passes to a separate adsorption train. The CIL arrangement keeps dissolved gold concentration very low, which maintains a steeper kinetic driving force and improves recovery on ores where dissolution is slow or where dissolved gold could be lost to re-precipitation. CIP can suit ores with fast leach kinetics, where the two stages can be separated without penalty.

6.2 How long should the leach residence time be?

Residence time should be set by leach test work kinetics rather than by a rule of thumb, because the time needed to reach target recovery varies widely between ores. Most gold cil leaching process circuits operate with a total residence time somewhere between 16 and 24 hours across the tank train. Faster-leaching ores need less, and ores containing slow-dissolving or partly refractory gold need more. The number of tanks and their individual volume follow directly from that figure and from the chosen pulp density.

6.3 Why does my cyanide consumption keep rising?

Consumption rises when something in the ore or the water is competing for cyanide. Copper minerals are the most common cause, forming their own cyanide complexes, and sulphides consume cyanide as they oxidise. Thiocyanate and other degradation products accumulate in recycled process water and add to the demand.

A rising trend should be investigated by measuring the copper and sulphide content of the feed and the chemistry of the process water. Correcting the water bleed often reduces consumption without any change to the ore.

6.4 How much carbon should be in each leach tank?

Most circuits run a carbon concentration between about 10 and 25 grams per litre, staged so that the earlier tanks carry more carbon than the later ones. The correct figure for a specific circuit is set by the adsorption isotherm for that ore and by the target tailings grade, not by convention. Carbon should be measured in each tank rather than assumed from the transfer rate, because screens block, transfer pumps wear and concentration drifts without any obvious alarm. A simple daily check against the design profile is enough to catch most problems early.

6.5 What causes carbon to lose adsorption capacity?

Two mechanisms dominate. Calcium carbonate and other salts precipitate onto the carbon surface and block pores, which is why an acid wash precedes elution. Organic compounds, including flotation reagents and oils, foul the surface and are removed by thermal regeneration in a kiln.

Mechanical attrition also reduces the particle size over time, and carbon fines are lost through the retention screens. Monitoring loading capacity and sizing the carbon periodically shows which mechanism is at work, and it lets the regeneration schedule be based on measured condition rather than on a fixed cycle.

The gold cil leaching process rewards attention to two variables that are easy to neglect: dissolved oxygen and carbon condition. Cyanide is dosed and measured routinely, while oxygen and carbon often are not, yet both can explain a persistent recovery gap. Measure both, keep the carbon clean and well regenerated, and operate the tank train so that pulp does not short-circuit. Henan Amill Machinery Equipment supplies gold cil leaching process circuits with agitation, aeration and carbon handling designed together, and our engineers support commissioning and operator training through the first months of operation.

Share

Contact Us

Send Inquiry to Us
* Message
0/5000

Want the best price? Post an RFQ now!

Recommended Products